Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K2GA5050A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K2GA5080A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® V2GA0065A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® V2GA1050d TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® V2GA1065A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® V5GA1090A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® V6GA3075A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Back Pressure 0.340 MPa
49.3 psi
Styrolution NAS® 90 High Performance Styrenic
NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K2GA4055D TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Back Pressure 0.340 MPa
49.3 psi
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins