Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Styrenic TPE
Manufacturer Termopol
Trade Name Termoton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance to heat, UV, O, and weathering; Excellent resistance to several chemical agents like bases, acids, alcohols, detergents etc; Transparency-easy coloring; Heat adhesion on rigid polymeric materials like PA, PC, ABS, PMMA, PS, SAN, TPU polymers; High elastic recovery within a wide temperature range; Soft rubbery touch, excellent wet and dry grip; Low compression set even at high temperature; High fatigue resistance; High thermal and electric insulation values; Good abrasion resistance; Many products meet FDA and REACH regulationsInformation provided by Termopol Termoplastik Elastomer
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 2781
Deformation 37 %

@Temperature 700 °C,
Time 79200 sec
37 %

@Temperature 1290 °F,
Time 22.0 hour
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
ISO 868
Tensile Strength 5.30 MPa
769 psi
ISO 37
Elongation at Break 600 %
600 %
ISO 37
100% Modulus 0.00190 GPa
0.276 ksi
ISO 37
300% Modulus 0.00260 GPa
0.377 ksi
ISO 37
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Nozzle Temperature 185 °C
365 °F
Zone 1 160 °C
320 °F
Zone 2 170 °C
338 °F
Zone 3 180 °C
356 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Drying Temperature 90.0 °C

@Time 7200 sec
194 °F

@Time 2.00 hour
Back Pressure 0.340 MPa
49.3 psi
Screw Speed 25 - 75 rpm
25 - 75 rpm
Descriptive Properties Value Comments
Acid-Base Resistance Excellent
Alcohol Resistance Excellent
Compression Set Good
Injection Pressure Medium
Injection Speed Medium-high
Motor Oil Resistance Medium
Plasticizing Speed High
Solvent Resistance Medium
UV-Ozone Stability Excellent