Processing Properties Metric English Comments
Back Pressure 0.700 - 1.10 MPa
102 - 160 psi
Hydraulic backpressure
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler
A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc.
Back Pressure 0.700 - 1.00 MPa
102 - 145 psi
Kingfa JH820 Modified PC
Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac..
Back Pressure 0.700 - 1.00 MPa
102 - 145 psi
Kingfa JH830T Flame Retardant PC
Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor..
Back Pressure 0.700 - 1.00 MPa
102 - 145 psi
Kingfa MAC-601 UV PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou..
Back Pressure 0.700 - 1.00 MPa
102 - 145 psi
Kingfa MAC-601 AC PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou..
Back Pressure 0.700 - 1.00 MPa
102 - 145 psi
Kingfa MAC-701 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p..