Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |