Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUCON PN9008 PPS+MF+GF Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Back Pressure | 0.981 - 1.96 MPa | 142 - 284 psi | Injection Molding |
LG Chemical LUMIPLAS LD590T Light diffusion ABS Description: Extrusion, Light diffusion, High ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
Back Pressure | 0.981 - 1.96 MPa | 142 - 284 psi | Injection Molding |
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC5004T PC/Polyester, Transparency Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 1.96 MPa | 142 - 284 psi | Injection Molding |
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, High Impact, Chemical ResistanceApplication: IT/OA (M/P Battery Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information prov.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000M PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1006FL PC, Flame Retardant Description: Injection Molding, PC, Flame Retardant, High FlowApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |