Material Notes:
Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene - Suitable for Outdoor UseDynaflex™ G7430-9001-00 can be recycled as a filler or impact modifier for polyolefins, or can be recycled by grinding and reintroduction to the molding process. Similar to PP or PE recycling process, if separated appropriately, it can be recycled many times. Municipality waste stream recycle code is 7 which is designated for Other. Please contact GLS Thermoplastic Elastomers for a copy of our Recyclability Compliance letter.Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Dynaflex™ G7430-9001-00 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt tempetature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 250 to 650 psi 2nd Stage - Hold Pressure: 50% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.918 g/cc
0.918 g/cc
ASTM D792
Viscosity 12600 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
12600 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
10 sec; ASTM D2240
Tensile Strength at Break 8.96 MPa

@Temperature 23.0 °C
1300 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 2.48 MPa

@Strain 100 %,
Temperature 23.0 °C
360 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
4.07 MPa

@Strain 300 %,
Temperature 23.0 °C
590 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 650 %

@Temperature 23.0 °C
650 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 36.8 kN/m
210 pli
ASTM D624
Compression Set 17 %

@Temperature 23.0 °C,
Time 79200 sec
17 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 168 - 177 °C
334 - 351 °F
Middle Barrel Temperature 177 - 188 °C
351 - 370 °F
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
Nozzle Temperature 188 - 227 °C
370 - 441 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 149 psi
Screw Speed 40 - 100 rpm
40 - 100 rpm
Descriptive Properties Value Comments
Appearance Black
Features Good Thermal Stability
Good UV Resistance
High Strength
Ozone Resistant
Recyclable Material
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Appliance Components
Consumer Applications
Overmolding
Sporting Goods
Strain Reliefs
Users viewing this material also viewed the following: