Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL TE-5202U Thermoplastic Elastomer Alloy, 20% Polymer Alloy, High Impact, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Back Pressure | 1.96 - 3.92 MPa | 284 - 569 psi | Injection Molding |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL FW-700A Friction and Wear Resistant POM, Polymeric Wear Additive LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL HF-3208H High Flow Polypropylene, 20% Mineral Fillers, General Purpose LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Back Pressure | 1.96 - 3.92 MPa | 284 - 569 psi | Injection Molding |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |