Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Back Pressure | 0.150 - 0.350 MPa | 21.8 - 50.8 psi | |
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |