Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Back Pressure = 29.0 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer
Information provided by Polykemi AB
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Polykemi AB POLYelast TPE R44 T10 Thermoplastic Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T6 GF30 (3501) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 1.00 MPa
29.0 - 145 psi
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture)
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
Back Pressure 0.200 - 1.00 MPa
29.0 - 145 psi
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 0.650 MPa
29.0 - 94.3 psi
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Back Pressure 0.200 - 1.00 MPa
29.0 - 145 psi
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
Back Pressure 0.200 - 1.00 MPa
29.0 - 145 psi
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
Back Pressure 0.200 - 1.00 MPa
29.0 - 145 psi
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..
Copyright © lookpolymers.com All Rights Reserved