Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Polykemi AB
Trade Name POLYelast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Index of Compound 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 55

@Time 15.0 sec
55

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 19.0 MPa
<= 2760 psi
ISO/R527
Elongation at Break 520 %
520 %
ISO/R527
Elongation at Yield 11 %
11 %
ISO/R527
Flexural Strength <= 27.0 MPa
<= 3920 psi
ISO 178
Flexural Modulus 1.15 GPa

@Temperature 23.0 °C
167 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
ISO 179
3.40 J/cm²

@Temperature 23.0 °C
16.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
120°C/h; ISO 75/1
Vicat Softening Point 130 °C

@Load 1.00 kg
266 °F

@Load 2.21 lb
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Mold Temperature 20.0 - 60.0 °C
68.0 - 140 °F
Injection Pressure 90.0 - 110 MPa
13100 - 16000 psi
Back Pressure 0.200 - 0.500 MPa
29.0 - 72.5 psi
Descriptive Properties Value Comments
Holding Pressure () 20-40
% of injection pressure
Injection Speed () High