Polymer Property : Screw Speed = 90 rpm Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® GP55 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® HF224 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® HF96 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® PL75 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® FR134 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® FR74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 50 - 90 rpm
50 - 90 rpm
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Screw Speed 30 - 90 rpm
30 - 90 rpm
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
Screw Speed 60 - 90 rpm
60 - 90 rpm
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Screw Speed 60 - 90 rpm
60 - 90 rpm
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).