Ravago Manufacturing Americas Hylac® GP55 ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylac® GP55 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 1.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
5.6 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.6 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Cond I; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 45.5 MPa
6600 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.52 GPa
365 ksi
ASTM D638
Flexural Yield Strength 70.3 MPa
10200 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 2.56 J/cm
4.80 ft-lb/in
0.25 in; ASTM D256
2.94 J/cm
5.50 ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 112 µm/m-°C

@Temperature -40.0 - 176 °C
62.0 µin/in-°F

@Temperature -40.0 - 349 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.2 °C
189 °F
Unannealed; ASTM D648
Vicat Softening Point 101 °C
213 °F
ASTM D1525
Flammability, UL94 HB
HB
0.0590 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Rear Barrel Temperature 179 - 199 °C
355 - 390 °F
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Front Barrel Temperature 216 - 235 °C
420 - 455 °F
Nozzle Temperature 210 - 229 °C
410 - 445 °F
Melt Temperature 241 °C
465 °F
Aim
Mold Temperature 48.9 - 60.0 °C
120 - 140 °F
Moisture Content <= 0.10 %
<= 0.10 %
Injection Pressure 5.86 - 6.89 MPa
850 - 1000 psi
Back Pressure 0.483 - 0.965 MPa
70.0 - 140 psi
Shot Size 40 - 80 %
40 - 80 %
Screw Speed 50 - 90 rpm
50 - 90 rpm
Descriptive Properties Value Comments
Holding Pressure 710 to 850 psi
Injection Rate Slow-Moderate