Polymer Property : Cure Time = 0.0250 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 0.333 - 1.50 min
0.00555 - 0.0250 hour
Time to Handling Strength
3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive
3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon..
Cure Time 1.00 - 1.50 min

@Temperature 150 °C
0.0167 - 0.0250 hour

@Temperature 302 °F
Loctite® CHIPBONDER® 3615 High Adhesion, Syringe Dispense
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..
Cure Time 1.00 - 1.50 min

@Temperature 150 °C
0.0167 - 0.0250 hour

@Temperature 302 °F
Loctite® CHIPBONDER® 3618 High Speed, Syringe Dispense
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..