Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1.33 - 2.00 min | 0.0222 - 0.0333 hour | On Steel (Fixture) |
ND Industries Toughened Ethyl SuperGlue 310 Black flexible Cyanoacrylate for metal, rubber, and plastic |
|||
Cure Time | 1.33 - 2.00 min | 0.0222 - 0.0333 hour | Metal set time |
Lord Adhesives 5181 High Viscosity, Black, General Purpose Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 1.00 - 2.00 min | 0.0167 - 0.0333 hour | |
3M Scotch-Weld™ CA50 Gel Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-viscosity, non-sag gel and less sensitive to acidic surfaces.Information provided by 3M |
|||
Cure Time | 1.50 - 2.00 min @Temperature 204 - 232 °C |
0.0250 - 0.0333 hour @Temperature 400 - 450 °F |
|
Unifrax Fiberfrax® Duraset® Flet Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i.. |