Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 15.0 - 18.0 min | 0.250 - 0.300 hour | working strength |
Permabond TA4820 Structural Acrylic Adhesive PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac.. |