Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5760 - 10080 min | 96.0 - 168.0 hour | For full cure. Maximum high temperature properties are obtained with a post cure of about 2 hours at 93°C to 121°C. |
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
(discontinued **) Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v.. |