Processing Properties Metric English Comments
Cure Time 5760 min

@Temperature 25.0 °C
96.0 hour

@Temperature 77.0 °F
Tra-Con Tra-Cast 3010 Flexible Clear Epoxy Casting Compound
TRA-CAST 3010 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life..
Cure Time 5760 min

@Temperature 25.0 °C
96.0 hour

@Temperature 77.0 °F
Tra-Con Tra-Cast 3011 Semi-Flexible Clear Epoxy Casting Compound
TRA-CAST 3011 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life..
Cure Time 5760 min

@Temperature 25.0 °C
96.0 hour

@Temperature 77.0 °F
Tra-Con Tra-Cast 3012 Clear Epoxy Casting Compound
TRA-CAST 3012 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties good clarity, long pot life,..
Cure Time 5760 - 7200 min
96.0 - 120 hour
(4-5 Days)
Abatron Epotron 5 Clear Liquid Epoxy Adhesive for Structural Bonding
Epotron 5 is a clear liquid epoxy adhesive for structural bonding. It is recommended for high-strength, permanent bonding of metal, ceramic, glass, laminates, and most rigid materials. Features: Hi..
Cure Time 5760 min
96.0 hour
Tack-Free Time
3M AC-236 Class C-80 Aerospace Sealant
3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance ..
Cure Time 5760 min
96.0 hour
Tack-Free Time
3M AC-350 Class B-12 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Cure Time 5760 min
96.0 hour
3M AC-350 Class B-12 Aerospace Sealant
3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are..
Cure Time 5760 min
96.0 hour
Tack-Free Time
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Cure Time 5760 min
96.0 hour
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Cure Time 5760 - 10080 min
96.0 - 168.0 hour
For full cure. Maximum high temperature properties are obtained with a post cure of about 2 hours at 93°C to 121°C.
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener  (discontinued **)
Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v..