Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
Roll Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Middle |
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Top |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Top |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical MU620 ABS, Low Deformation Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical SH610A ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical SH610A ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle, Extrusion |
LG Chemical SH610S ABS, Excellent Surface, High Impact Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Middle |
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Roll Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Middle |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Middle |
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Roll Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Middle |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Roll Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Middle |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |