Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-15 Polyester SMC Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2103-22 CRSX Polyester BMC Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-20 CRSX Polyester SMC Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1281-47 VE SMC Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |