Processing Properties | Metric | English | Comments |
---|---|---|---|
Cycle Time - Cooling | 30 sec | 30 sec | |
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude.. |
|||
Cycle Time - Cooling | 30 sec | 30 sec | |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist.. |