Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 0.167 - 0.333 min | 0.167 - 0.333 min | 400 watt UV |
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas.. |
|||
Gel Time | 0.167 - 0.200 min | 0.167 - 0.200 min | |
Dow SPECTRIM™ MM310 Reaction Moldable Polymer SPECTRIM™ MM 310 reaction moldable polymer is a three-component, fast-reacting, low viscosity polycarbamate system ideally suited for mat molding of structural composites. The structural reaction .. |