Processing Properties Metric English Comments
Gel Time 3.00 - 20.0 min

@Temperature 23.9 °C
3.00 - 20.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EcoWIND® 200 Polyurethane Resin Filament Winding  (discontinued **)
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Gel Time 16.0 - 20.0 min
16.0 - 20.0 min
Value for a 100g mass, catalyzed at 2 percent with MEKP - 2%
Fibre Glast Duratec 1040 Clear Hi-Gloss Gel Coat Additive
#1040 can be mixed 1:1 with regular gel coat to reduce viscosity, porosity, and permit a complete open air cure. The reduction in viscosity allows gel coat to be sprayed controllably through siphon ..
Gel Time 3.00 - 20.0 min

@Temperature 23.9 °C
3.00 - 20.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Gel Time 3.00 - 20.0 min

@Temperature 23.9 °C
3.00 - 20.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Copyright © lookpolymers.com All Rights Reserved