Processing Properties Metric English Comments
Gel Time 3.00 - 4.00 min
3.00 - 4.00 min
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced
Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s..
Gel Time 3.00 - 30.0 min

@Temperature 135 °C
3.00 - 30.0 min

@Temperature 275 °F
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4503 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Gel Time 3.00 - 30.0 min

@Temperature 135 °C
3.00 - 30.0 min

@Temperature 275 °F
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Gel Time 3.00 - 5.00 min
3.00 - 5.00 min
Resin Technology Group 1121 Two component Polyurethane Adhesive
Resin Technology Group 1121 Two component Polyurethane AdhesiveMedium viscosity, clear, Lexan bonding adhesive
Gel Time 3.00 - 15.0 min

@Temperature 23.9 °C
3.00 - 15.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding  (discontinued **)
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Gel Time 3.00 - 20.0 min

@Temperature 23.9 °C
3.00 - 20.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EcoWIND® 200 Polyurethane Resin Filament Winding  (discontinued **)
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Gel Time 3.00 - 18.0 min
3.00 - 18.0 min
when reacted at 1:1 by volume, based on the application
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Gel Time 3.00 min

@Temperature 150 °C
3.00 min

@Temperature 302 °F
Lord Adhesives Circalokâ„¢ EP-937 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ EP-937 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by..
Gel Time 3.00 - 5.00 min

@Temperature 150 °C
3.00 - 5.00 min

@Temperature 302 °F
Lord Adhesives Thermosetâ„¢ ME-455 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ ME-455 encapsulant is a onecomponent, semiconductor grade epoxy designed for the encapsulation of wire-bonded or flip chip die in PPGA, BGA, MCM and other cavity packages. It is..
Gel Time 3.00 min

@Temperature 150 °C
3.00 min

@Temperature 302 °F
Lord Adhesives Thermosetâ„¢ ME-541 Underfill Encapsulant
LORD Thermosetâ„¢ ME-541 encapsulant is an anhydride free, high purity, semi-conductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip chip devi..
Gel Time 3.00 min

@Temperature 150 °C
3.00 min

@Temperature 302 °F
Lord Adhesives Thermosetâ„¢ ME-542 Underfill Encapsulant
LORD Thermosetâ„¢ ME-542 encapsulant is an anhydridefree, thermally conductive, semiconductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip ch..
Gel Time 3.00 - 18.0 min
3.00 - 18.0 min
when reacted at 1:1 by volume, based on the application
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Gel Time 3.00 - 15.0 min

@Temperature 23.9 °C
3.00 - 15.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EzNATE® 100 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Gel Time 3.00 - 20.0 min

@Temperature 23.9 °C
3.00 - 20.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Gel Time 3.00 min
3.00 min
ACC QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
QGel 311 is a clear, fast cure, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
Gel Time 3.00 - 15.0 min

@Temperature 23.9 °C
3.00 - 15.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EzNATE® 100 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Gel Time 3.00 - 20.0 min

@Temperature 23.9 °C
3.00 - 20.0 min

@Temperature 75.0 °F
when reacted at 1:1 by volume, based on application
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..