Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 240 min @Temperature 25.0 °C |
240 min @Temperature 77.0 °F |
Thin Film |
Trelleborg Emerson & Cuming EP578 Adhesive Density matched blue adhesive for use with EP678, TB610 and TB620.All information provided by Trelleborg Emerson & Cuming |
|||
Gel Time | 240 min @Temperature 25.0 °C |
240 min @Temperature 77.0 °F |
Thin Film |
Trelleborg Emerson & Cuming EP646 Patch Paste Filled patch system or EP671 boardAll information provided by Trelleborg Emerson & Cuming |