Processing Properties Metric English Comments
Gel Time 25.0 - 30.0 min
25.0 - 30.0 min
Value for 4 fl. oz.; ASTM D2471
Fibre Glast 1100 Light-Weight High-Strength Patching/Filler Compound
Product Features:Very Light Weight MaterialNon-Hazardous Product - Safe to UseEasily Sanded and Carved with Shop ToolsNegligible ShrinkageNon-Critical, 2 to 1 Ratio by Weight or by VolumeExcellent N..
Gel Time 25.0 min
25.0 min
Loctite® 3171 Deep Potting Polyurethane
PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies.For e..