Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 1.00 Month @Temperature 4.44 °C |
1.00 Month @Temperature 40.0 °F |
|
Quantum Composites HTC-9500 55% E-Glass Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9500 (127-51-6) is an E-Glass Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics providing .. |
|||
Shelf Life | 1.00 Month @Temperature 4.44 °C |
1.00 Month @Temperature 40.0 °F |
|
Quantum Composites HTC-9590 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9590 (127-51-3) is a 12K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristic.. |
|||
Shelf Life | 1.00 Month @Temperature 4.44 °C |
1.00 Month @Temperature 40.0 °F |
|
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9593 (127-51-5) is a 3K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics.. |
|||
Shelf Life | 1.00 Month @Temperature 23.0 °C |
1.00 Month @Temperature 73.4 °F |
|
Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix HexPly® M14 is a modified epoxy resin which provides good adhesion to honeycomb and foam cores. Its self-extinguishing characteristics meet the fire, smoke, and toxicity requirements of aerospace a.. |
|||
Shelf Life | 1.00 Month @Temperature 23.0 °C |
1.00 Month @Temperature 73.4 °F |
|
Hexcel® HexPly® M27 248°F (120°C) Curing Epoxy Matrix HexPly® M27 is specifically designed for applications with fast curing cycles. It is ideally suited for high volume production techniques-in particular for ski manufacture. HexPly® M27 has been sp.. |