Processing Properties Metric English Comments
Pot Life 16 - 24 min

@Temperature 60.0 - 80.0 °C
16 - 24 min

@Temperature 140 - 176 °F
Abatron AboCast/AboCure 7606-1 Epoxy
AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight o..