Processing Properties Metric English Comments
Melt Temperature 124 - 280 °C
255 - 536 °F
Average value: 207 °C Grade Count:57
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Melt Temperature 124 °C
255 °F
Iran Petrochemical (PCC) MF3313 High Density Polyethylene
MF3313 is a high molecular weight high density polyethylene . Applications: extrusion, film, blown, bags, and density modifies.Information provided by Iran Petrochemical Commercial Co.
Melt Temperature >= 124 °C
>= 255 °F
Borealis Polycure™ PC531 Track Resistant Crosslinking Polyethylene Compound for Overhead Cable Insulation
Polycure PC531 is a black, chemically crosslinking polyethylene compound that is designed for use in track resistant overhead cable insulation and jacketing.Polycure PC531 is suitable for use in pow..
Melt Temperature 124 - 321 °C
255 - 610 °F
Average value: 216 °C Grade Count:35
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..