Processing Properties Metric English Comments
Melt Temperature 127 °C
261 °F
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene
LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co.
Melt Temperature 127 °C
261 °F
Borealis PC0798 Polyethylene Insulation Compound, Crosslinkable
PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retar..