Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 127 °C | 261 °F | |
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Temperature | 127 °C | 261 °F | |
Borealis PC0798 Polyethylene Insulation Compound, Crosslinkable PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retar.. |