Polymer Property : Melt Temperature = 318 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 288 - 318 °C
550 - 604 °F
Extrusion
Albis Plastics Tedur® L V 9112-2 PPS, 20% Glass Fiber  (discontinued **)
Excellent Surface Finish (Additional Annealing May Be Necessary). Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pipes, ProfilesProcessing: Extrusion (Melt Temperatur..