Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 288 - 318 °C | 550 - 604 °F | Extrusion |
Albis Plastics Tedur® L V 9112-2 PPS, 20% Glass Fiber
(discontinued **) Excellent Surface Finish (Additional Annealing May Be Necessary). Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pipes, ProfilesProcessing: Extrusion (Melt Temperatur.. |