Polymer Property : Melt Temperature = 370 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 340 - 370 °C
644 - 698 °F
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Melt Temperature 350 - 370 °C
662 - 698 °F
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Melt Temperature 350 - 370 °C
662 - 698 °F
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Melt Temperature 340 - 370 °C
644 - 698 °F
LATI Lapex A PES
Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Melt Temperature 350 - 370 °C
662 - 698 °F
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Melt Temperature 350 - 370 °C
662 - 698 °F
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Melt Temperature 360 - 370 °C
680 - 698 °F
E-Polymers SEPAZ® C240GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Melt Temperature 360 - 370 °C
680 - 698 °F
E-Polymers SEPAZ® C245GP 45% Glass Fiber Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..