Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid) Physical properties based on Geon L6607 white 1363Information provided by PolyOne |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable EMB405L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable EMB405LU Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2407L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable W3201 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon® W3201 is UL recognized for UL 94 V0 per QMFZ2, and is suitable for injection molding. This product meets UL 105°C, AWM, and Mil-W-76 80°C insulation.NOTE: Typical Properties of Molded Slab .. |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable W780L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable W9400 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable W9400L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable WEMB410 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable WEMB410U Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 188 °C | 340 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJC340U Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Flexible B8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Flexible FC700 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Flexible G92D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Flexible R109AM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Flexible R296CM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 188 °C | 340 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJC340 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 179 - 188 °C | 354 - 370 °F | |
PolyOne Geon™ Vinyl Flexible 86479 Natural Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 188 °C | 354 - 370 °F | |
PolyOne Geon™ Vinyl Flexible 86479 Opaque Polyvinyl Chloride Information provided by PolyOne |
|||
Melt Temperature | 179 - 188 °C | 354 - 370 °F | |
PolyOne Geon™ Vinyl Flexible 86479 Tran Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Flexible G92C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 188 °C | 354 - 370 °F | |
PolyOne Geon™ Vinyl Flexible R336AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Flexible R349AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 182 - 188 °C | 360 - 370 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2407 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |