Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 sec; ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 182 - 188 °C
360 - 370 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Additive Biocide
UV Stabilizer
Features General Purpose
High Gloss
UV Absorbing
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Flooring
General Purpose
Outdoor Applications