Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 65.0 - 125 °C | 149 - 257 °F | |
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |