Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.800 mm |
7.0 - 15 sec @Thickness 0.0315 in |
UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.800 mm |
7.0 - 15 sec @Thickness 0.0315 in |
UL 746 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=2.00 mm |
7.0 - 15 sec @Thickness >=0.0787 in |
|
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=2.50 mm |
7.0 - 15 sec @Thickness >=0.0984 in |
|
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=3.00 mm |
7.0 - 15 sec @Thickness >=0.118 in |
|
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.710 mm |
7.0 - 15 sec @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 3.00 mm |
7.0 - 15 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.710 mm |
7.0 - 15 sec @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.710 mm |
7.0 - 15 sec @Thickness 0.0280 in |
UL 746A |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 1.50 mm |
7.0 - 15 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 3.00 mm |
7.0 - 15 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |