Hot Wire Ignition, HWI 39 sec

@Thickness 1.47 mm
39 sec

@Thickness 0.0580 in
UL 746A
Glastic SG-200 Industrial Lift Magnet
Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature ..