Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc Resistance to Ignition (HVAR) | 150 sec | 150 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |