Electrical Properties Metric English Comments
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17500)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 10 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17500)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17510)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 3 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17510)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 3 Tube; HT (TH04) Temper; up to 76 mm o.d. (UNS C17510)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc...
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 3 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials ..
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity
Materion Beryllium Copper Alloy 3 Strip; HT (TH04) Temper (UNS C17510)
Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 75%Formability Ratio..