Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17510)

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17510).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.83 g/cc
0.319 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 95 - 102
95 - 102
Tensile Strength, Ultimate 750 - 970 MPa
109000 - 141000 psi
Tensile Strength, Yield 680 - 830 MPa
98600 - 120000 psi
Elongation at Break 5.0 - 15 %
5.0 - 15 %
Modulus of Elasticity 138 GPa
20000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 240 W/m-K
1670 BTU-in/hr-ft²-°F
Melting Point 1040 - 1080 °C
1900 - 1980 °F
Solidus 1040 °C
1900 °F
Liquidus 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.20 - 0.60 %
0.20 - 0.60 %
Copper, Cu 98 %
98 %
as balance
Nickel, Ni 1.4 - 2.2 %
1.4 - 2.2 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000290 - 0.00000360 ohm-cm
0.00000290 - 0.00000360 ohm-cm
48-60% IACS Conductivity