Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 10 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Electrical Resistivity | 0.00000340 - 0.00000380 ohm-cm | 0.00000340 - 0.00000380 ohm-cm | 45-50% IACS Conductivity |
Materion Beryllium Copper Alloy 10C Castings (UNS C82000) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 174 Strip; 1/2HT (TH02) Temper (UNS C17410) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; AT (TF00) Temper (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials .. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; AT (TF00) Temper (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Strip; AT (TF00) Temper (UNS C17510) Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 94%Stress Relaxation after 1000 hrs @ 200°C: 72%Formability Ratio.. |
|||
Electrical Resistivity | 0.00000290 - 0.00000380 ohm-cm | 0.00000290 - 0.00000380 ohm-cm | 45-60% IACS Conductivity |
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |