Electrical Resistivity 0.00000340 ohm-cm
0.00000340 ohm-cm
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite
RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is ..
Electrical Resistivity 0.00000340 ohm-cm
0.00000340 ohm-cm
Hogen H20S, 26 Silver/74 Tungsten PM Metal Composite
RWMA Class EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica..
Electrical Resistivity 0.00000340 - 0.00000380 ohm-cm
0.00000340 - 0.00000380 ohm-cm
45-50% IACS Conductivity
Materion Beryllium Copper Alloy 10C Castings (UNS C82000)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul..
Electrical Resistivity <= 0.00000340 ohm-cm
<= 0.00000340 ohm-cm
50% IACS conductivity (minimum)
Materion Brush 60â„¢ HT
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte..
Electrical Resistivity 0.00000340 ohm-cm
0.00000340 ohm-cm
Mi-Tech Metals CW68 68 Tungsten/32 Copper PM Metal Composite
RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme..
Electrical Resistivity 0.00000340 ohm-cm
0.00000340 ohm-cm
Mi-Tech Metals SW74 26 Silver/74 Tungsten PM Metal Composite
RWMA Class EDMMi-Tech Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Chemica..
Electrical Resistivity <= 0.00000340 ohm-cm
<= 0.00000340 ohm-cm
50% IACS conductivity (minimum)
Materion Brush 60â„¢ 3/4 HT
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte..
Electrical Resistivity 0.00000340 ohm-cm
0.00000340 ohm-cm
Temper T651
Constellium DOKIMA® Rolled Plate Aluminum
DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conduct..
Electrical Resistivity 0.00000340 ohm-cm
0.00000340 ohm-cm
51 % IACS
CMW® ELKONITE 35SB tungsten, silver
ELKONITE® 35SB is the most popular material made by the press sinter process with a small addition of nickel used to activate the sintering. Because of fewer steps in manufacture this material is m..