Electrical Resistivity 0.00000520 ohm-cm
0.00000520 ohm-cm
33 % IACS
CMW® ELKON 100M Pure Molybdenum
Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The elec..