Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000573 ohm-cm | 0.00000573 ohm-cm | Calculated from 30 %IACS |
Cadi 100M Molybdenum Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |
|||
Electrical Resistivity | 0.00000573 - 0.00000688 ohm-cm | 0.00000573 - 0.00000688 ohm-cm | Calculated from 25-30 %IACS |
Cadi 10WA Tungsten Copper Alloy Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |