Polymer Property : Electrical Resistivity = 0.00000639 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm
Pacific Sintered Materials BZ-111-UC Yellow Brass Powdered Metal
Applications: 80-20 leaded brass, coined for close dimensional control, strength and density.Equivalent MPIF Specification: CZP-2000-12All information provided by Pacific Sintered Metals.
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy
Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extrude..
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy
Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm
Chicago Extruded Metals UNS C37700 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, M30Information provided by Chicago Extruded Metals