Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 - 0.0000101 ohm-cm
0.00000748 - 0.0000101 ohm-cm
Conductivity is 17-23% IACS
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
Electrical Resistivity 0.00000748 ohm-cm
0.00000748 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
California Fine Wire Nickel 220 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Electrical Resistivity 0.00000748 ohm-cm
0.00000748 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
California Fine Wire Nickel 271 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Electrical Resistivity 0.00000748 ohm-cm
0.00000748 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
California Fine Wire Nickel 272 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Electrical Resistivity 0.00000748 ohm-cm
0.00000748 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
California Fine Wire Nickel 5900 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.