California Fine Wire Nickel 5900 Nickel Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Pure Element
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Nickel 5900 Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 345 MPa
50000 psi
Annealed
552 MPa
80000 psi
Stress relieved
689 MPa
100000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 59.0 W/m-K
409 BTU-in/hr-ft²-°F
Melting Point 1450 °C
2642 °F
Maximum Service Temperature, Air 932 °C
1710 °F
Operating Temperature
Component Elements Properties Metric English Comments
Nickel, Ni 99.98 %
99.98 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000748 ohm-cm
0.00000748 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.0059 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.022