Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000118 ohm-cm | 0.0000118 ohm-cm | |
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
Electrical Resistivity | 0.0000118 ohm-cm | 0.0000118 ohm-cm | |
Carlson C 201 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |