Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Parkway Products Thixomolded® AM50A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Hogen Diemitechâ„¢ Tungsten-Based Metal Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available.. |
|||
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Hogen HM1000 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offe.. |
|||
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Hogen HM1250 Tungsten-Based Metal Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduce.. |
|||
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Mi-Tech Metals Diemitechâ„¢ Tungsten-Based Metal Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available.. |
|||
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Mi-Tech Metals HD17 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. .. |
|||
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Mi-Tech Metals HD17BB Tungsten-Based Metal ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t.. |
|||
Electrical Resistivity | 0.0000120 ohm-cm | 0.0000120 ohm-cm | |
Mi-Tech Metals Super Chatter Freeâ„¢ HD17.7 Tungsten-Based Metal Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduce.. |